PRODUCT SUMMARY:

Wonstar Crack seal structural adhesive, sold in Sri Lanka by Onyx Engineering, is a two-component modified epoxy resin paste adhesive, often used in crack sealing and waterproof engineering. It can effectively solve the problem of cracks on the surface of concrete, glass fiber reinforced plastic, wood and other materials. It is widely used in hydraulic engineering, construction engineering, bridge engineering and other fields.

Product Features

  • Strong adhesion.
  • Good thixotropy.
  • Strong durability.
  • Fast curing.
  • Similar color.
  • Environmental friendly and non-toxic.
  • This product is safe and non-toxic, non-dangerous goods, which can be transported according to general chemical building materials


GENERAL SPECIFICATIONS:

 

 Key Details
Brand Wonstar
Type Crack Seal Adhesives
Model Number WSD-30FF
Primary Material Epoxy Resin
Colour Component A: White paste
Component B: Grey past
After Mixing: Grey past
Volume 390ml
Proportioning 3:1
Usage Approximately 1 kg of adhesive is used for every 3-5 meter long crack.
Curing Time 1-2 days.
*Refer product manual for details.
Applications Crack sealing
Defect repair
Edge sealing treatment
Anti-corrosion construction

 

 Technical Parameters
Testing Items Testing Conditions Qualification Criteria
(GB50728-2011) Class I
Colloidal
Performance
Tensile Strength (MPa) Under conditions of (23±2)°C and (50±5)% relative
humidity, the test is conducted at a loading rate of 2mm/min.
≥30
Tensile Elastic Modulus (MPa) ≥1.5×10³
Elongation (%) ≥1.5
Bending Strength (MPa) ≥40, and no fracture
failure is allowed
Compressive Strength (MPa) ≥70
Adhesion
Performance
Steel-steel (steel sleeve) tensile
anti-shear strength (MPa)
(23±2)°C、(50±5)%RH ≥10
Steel-steel adhesive tensile
strength (MPa)
At (23±2)°C and (50±5)% RH, the test is
conducted according to the specified loading
speed as per the test method standard.
≥32
Steel-steel T impact stripping
length (mm)
≤35
  Steel-concrete Tensile
Strength (MPa)
≥2.5, and cohesive failure
within the concrete
Heat distortion temperature (°C) Using method B with a bending stress ≥65
Non-volatile Content (%) (105±2)°C、(180±5)min ≥99
Seraphinite AcceleratorOptimized by Seraphinite Accelerator
Turns on site high speed to be attractive for people and search engines.